Lubricants are used in reduction of the tubing on the OD and ID, and is then degreased in preparation for annealing. Usually this method generates lengths after reduction from around 40 feet to 160 feet in total. Cold reduction is the most effective process for the development of long stretches of smooth tubing in a coil shape.